Monel 400 vs Monel K-500: Differences, Properties and Uses

Monel 400 (UNS N04400) vs Monel K-500 (UNS N05500): composition, strength, age hardening, ASTM B164 and B865 bar specifications, and when to use each alloy.

By JPS Metal & Alloys · 19 Nov 2026 · 5 min read

Monel 400 (Alloy 400, UNS N04400) and Monel K-500 (Alloy K500, UNS N05500) are nickel-copper alloys known for their resistance to seawater, hydrofluoric acid and alkalis. They share almost the same base composition, so their corrosion resistance is similar. The difference is strength: K-500 can be age hardened, Monel 400 cannot.

Composition

ElementMonel 400 (N04400)Monel K-500 (N05500)
Nickel (%)63.0 min63.0 min
Copper (%)28.0 to 34.027.0 to 33.0
Aluminium (%)—2.30 to 3.15
Titanium (%)—0.35 to 0.85
W.Nr.2.4360 (NiCu30Fe)2.4375 (NiCu30Al)
Bar specificationASTM B164ASTM B865

Strength and hardening

Monel 400 is a single-phase solid-solution alloy. It can be strengthened by cold working but not by heat treatment. K-500 adds aluminium and titanium, which form fine precipitates during an ageing heat treatment. After age hardening, K-500's yield strength is several times that of annealed Monel 400. That makes it suitable for heavily loaded parts that also need nickel-copper corrosion resistance.

The trade-off is toughness and ductility. Monel 400 is tougher and easier to form, and it keeps good impact properties at sub-zero temperatures. Both alloys work harden quickly, so machine them with sharp tools, rigid set-ups and steady feeds. K-500 is usually rough-machined before ageing and finish-machined after.

Corrosion resistance

Corrosion resistance is broadly the same for both grades in seawater, brackish water, hydrofluoric acid and caustic service. For sour (H2S) oil and gas service, check the hardness limits in NACE MR0175 / ISO 15156 before specifying age-hardened K-500.

Typical applications

  • Monel 400: marine and seawater piping, valves and pump bodies, HF alkylation units in refineries, heat exchangers, chemical process equipment and springs.
  • Monel K-500: pump shafts, propeller shafts, valve stems and trim, impellers, high-strength fasteners, springs, subsea components and oil-tool parts. It is also used where high strength and low magnetic permeability are needed together.

Monel 400 or K-500: how to choose

Specify Monel 400 when corrosion resistance is the main requirement and loads are moderate, for example in piping, valve bodies and vessels. Specify K-500 when a part must carry high loads or resist wear in the same corrosive environment, such as shafts, stems and fasteners. Always state the condition you need (annealed, hot-finished or age-hardened) and the hardness or strength range on the purchase order.

Monel bars from JPS Metal & Alloys

We supply Monel 400 round bars to ASTM B164 and Monel K-500 bars to ASTM B865, in a range of diameters, with EN 10204 3.1 mill test certificates. Bars can be cut to size or machined into finished shafts. Send your size, condition and quantity for a quote.

Frequently Asked Questions

Is Monel 500 the same as Monel K-500?
Yes. 'Monel 500' is a common short name for Monel K-500, also called Alloy K500, UNS N05500, W.Nr. 2.4375.
Which is stronger, Monel 400 or K-500?
K-500. After age hardening, its yield strength is several times that of annealed Monel 400, while its corrosion resistance stays broadly similar.
Can Monel 400 be heat treated to increase strength?
No. Monel 400 can only be strengthened by cold working. If you need higher strength, specify age-hardened Monel K-500.