Seawater is a difficult environment: it is full of chlorides, it supports marine growth and it can be warm and fast moving. Material choice depends on temperature, flow velocity and how long the system must last.
| Material | Strengths | Limits |
|---|---|---|
| SS 316L | Low cost, easy to fabricate | Pitting and crevice corrosion in warm or stagnant seawater, so limited to splash and cold, flowing water |
| Duplex 2205 | High strength, good chloride resistance | Can pit in warm, stagnant seawater |
| Super duplex 2507 | PREN above 40, high strength, widely used offshore | Needs controlled welding |
| Cupro-nickel 90/10 and 70/30 | Natural resistance to biofouling, long history in marine piping and condensers | Flow velocity limits, sensitive to sulphide-polluted water |
| Titanium Gr. 2 | Essentially immune to seawater corrosion | Higher initial cost, galvanic effects with other metals |
Marine growth and biofouling
Cupro-nickel releases copper ions at the surface, which discourages the growth of barnacles and algae. Stainless steels and titanium do not, so they usually need chlorination or other antifouling methods.
Galvanic corrosion
Connecting different metals in seawater can speed up corrosion of the less noble one. Match flange, bolt and pipe materials, or electrically isolate the joints.
Practical guidance
- Offshore and subsea piping, flanges and fasteners: super duplex 2507.
- Ship piping, condensers and heat exchangers: 90/10 or 70/30 cupro-nickel.
- Plate heat exchangers and critical chloride equipment: titanium Gr. 2.
- Coastal, non-immersed equipment: SS 316L.