Flange joints depend on correct stud bolts and nuts. The bolt grade sets the clamping load and the nut grade must match it, otherwise the nut can strip before the stud yields.
| Stud grade | Material | Typical nut | Used for |
|---|---|---|---|
| A193 B7 | Chromium-molybdenum alloy steel, quenched and tempered | A194 2H | General high-temperature and high-pressure service |
| A193 B7M | Same, controlled to lower hardness | A194 2HM | Sour service under NACE MR0175 |
| A193 B16 | Chromium-molybdenum-vanadium steel | A194 4 or 7 | Higher temperature service |
| A193 B8 / B8M | 304 / 316 stainless | A194 8 / 8M | Corrosive, low-temperature and marine service |
| A320 L7 | Alloy steel with impact testing | A194 4 or 7 | Low-temperature service |
B7 vs B8M
B7 is much stronger, with a minimum tensile strength of 125 ksi against about 75 ksi for B8M Class 1, but it rusts without a coating. B8M resists corrosion on its own. Strain hardened B8M Class 2 increases strength while keeping the corrosion resistance.
Coatings
- PTFE or Xylan coating: low friction and good corrosion protection for B7 studs.
- Hot dip galvanizing: low-cost corrosion protection for outdoor structures.
- Zinc plating: light protection for indoor and mild service.
Ordering checklist
State the stud grade, diameter, thread pitch, overall length, nut grade, coating and the number of nuts per stud (normally two). We supply stud bolts in carbon, alloy, stainless, duplex and nickel alloys, cut and threaded to your requirement.