Nickel alloys fill the gap where stainless steel fails because of acid, chloride, heat or strength demands. These three are among the most specified grades, and each one solves a different problem.
| Property | Inconel 625 (N06625) | Inconel 718 (N07718) | Hastelloy C276 (N10276) |
|---|---|---|---|
| Nickel (%) | 58 min | 50 to 55 | balance (about 57) |
| Chromium (%) | 20 to 23 | 17 to 21 | 14.5 to 16.5 |
| Molybdenum (%) | 8 to 10 | 2.8 to 3.3 | 15 to 17 |
| Other key elements | Nb 3.15 to 4.15 | Nb 4.75 to 5.5, Ti, Al | W 3 to 4.5 |
| Strengthening | Solid solution | Precipitation hardening | Solid solution |
| Main strength | Corrosion and fatigue | Very high strength to about 650 C | Acid and chemical resistance |
Inconel 625
Inconel 625 combines strong pitting and crevice resistance with good weldability and strength without heat treatment. It is widely used for seawater piping, flexible hoses, bellows, flare tips, heat exchanger tubing and as a corrosion-resistant weld overlay.
Inconel 718
Inconel 718 is age hardened to reach very high yield strength while keeping toughness. It is the standard for downhole tools, wellhead components, high-strength fasteners and gas turbine parts, and is commonly supplied to API 6A 718 and NACE MR0175 requirements.
Hastelloy C276
Hastelloy C276 resists both oxidizing and reducing acids, wet chlorine and chloride solutions. It is used in flue gas desulphurization, chemical reactors, pulp bleaching and pharmaceutical processing.
How to choose
- Seawater, chloride stress cracking and general corrosion plus fabrication: Inconel 625.
- High strength oil and gas tools, fasteners and shafts: Inconel 718.
- Aggressive acids and mixed chemical streams: Hastelloy C276.
We supply all three as round bars, plates, pipes, fittings, flanges and fasteners with 3.1 certificates and PMI on request.