JPS METAL & ALLOYS/ISO 9001:2015 CERTIFIED/MUMBAI, INDIA
VEDAANT@JPSMETAL.IN/+91 22 66630010
IndustriesContact UsBlogAbout

Duplex 2205 vs Super Duplex 2507: Which One Should You Specify?

Compare duplex 2205 (UNS S32205 / S31803) and super duplex 2507 (UNS S32750): composition, PREN, strength, temperature limits and typical applications.

By JPS Metal & Alloys · 15 Sep 2026 · 5 min read

Duplex stainless steels have a mixed structure of austenite and ferrite. That structure gives roughly double the yield strength of 304 or 316 together with much better resistance to chloride stress corrosion cracking. Duplex 2205 is the standard grade; super duplex 2507 adds chromium, molybdenum and nitrogen for harsher service.

Composition and PREN

PropertyDuplex 2205 (S32205)Super Duplex 2507 (S32750)
Chromium (%)22.0 to 23.024.0 to 26.0
Nickel (%)4.5 to 6.56.0 to 8.0
Molybdenum (%)3.0 to 3.53.0 to 5.0
Nitrogen (%)0.14 to 0.200.24 to 0.32
PREN (typical)about 3540 or higher
Min. yield strength (ASTM A240)450 MPa550 MPa
Min. tensile strength (ASTM A240)655 MPa795 MPa

PREN, the pitting resistance equivalent number, is calculated as Cr + 3.3 x Mo + 16 x N. A higher number means better resistance to pitting. Super duplex is defined by a PREN of 40 or more.

Temperature limits

Both grades lose toughness above about 300 degrees Celsius because of 475 degree embrittlement, and they should not be held in the sigma phase range. Most design codes limit duplex to roughly 250 to 300 degrees Celsius. For higher temperatures use austenitic stainless or nickel alloys instead.

Typical applications

  • Duplex 2205: pressure vessels, chemical tankers, heat exchangers, pulp and paper, desalination, process piping.
  • Super duplex 2507: subsea manifolds, offshore seawater systems, flanges and fasteners, high-chloride process lines, pumps and valves.

Welding and fabrication

Both grades need controlled heat input and matching or over-alloyed filler to keep the ferrite and austenite balance. Super duplex is less forgiving, so qualified procedures and ferrite checks are standard on critical jobs. Specify ASTM A790 or A789 for pipe and tube, ASTM A182 F51, F53 or F55 for flanges and fittings, and ASTM A240 for plate.

Need material to a specification? Send your grade, size and quantity.

Request a Quote →